Heat treatment
Quench and temper, normalising, stress relief and case hardening in furnaces surveyed to AMS 2750.

02Service

Shafts, rings, discs and blocks up to 18 t, forged on a 2,500 t press from ingots we melt ourselves.
Because the ingot is poured in our own melt shop, the heat number, chemistry and cleanliness data carry straight through to the forging. Reduction ratios and forging temperatures are logged for every piece.
Most forgings leave rough or finish machined, heat treated and ultrasonically tested, with one certificate covering the whole route.
Forgings start from ingots poured here, so the melt record carries through.
Forging ratio and temperatures are logged for every heat and every piece.
Every forging is ultrasonically tested to EN 10228-3 before it ships.


At least 3:1 on shafts and 4:1 where the standard or your drawing requires it, recorded per piece.
Yes. Most forgings leave rough or finish machined, heat treated and UT tested.
We prefer our own melt for traceability, but we can forge supplied material when it comes with its certificates.